SRD-100 microcomputer-controlled electronic creep tester can perform tensile, creep, long-lasting and stress relaxation tests on metal non-metal materials under certain temperature conditions, and can also perform low cycle fatigue and creep fatigue tests. Mainly used in the measurement of quality inspection, aerospace, metallurgical steel, colleges and universities and research laboratories and other industrial sectors.
SRD-100 microcomputer-controlled electronic creep tester can perform tensile, creep, long-lasting and stress relaxation tests on metal non-metal materials under certain temperature conditions, and can also perform low cycle fatigue and creep fatigue tests. Mainly used in the measurement of quality inspection, aerospace, metallurgical steel, colleges and universities and research laboratories and other industrial sectors.
|
Serial number |
project name |
Technical Parameters |
|
1 |
Maximum test force (kN) |
100 |
|
2 |
level of accuracy |
0.5 level / 1 level |
|
3 |
Test force measurement range |
1% to 100% FS |
|
4 |
Test force relative value |
±0.5%/±1% |
|
5 |
Test force resolution |
1/240000 (no change in the whole range) |
|
6 |
Concentricity |
≤10% |
|
7 |
Deformation measurement error |
±0.002mm (grating sensor) |
|
8 |
Pull rod maximum stroke |
150mm |
|
9 |
Tie rod speed |
0.01~50mm/min |
|
10 |
Mainframe dimensions (length × width × height) mm |
820×500×2360 |
|
11 |
Host weight (kg) |
520 |
|
12 |
Temperature range (°C) |
200~1100 |
|
13 |
Temperature fluctuation (°C) |
±2 |
|
14 |
Average tropical length (mm) |
150 |
|
15 |
Temperature gradient (°C) |
3 |




Dijawab otomatis oleh AI. Untuk detail, chat tim kami di WhatsApp.
Portfolio
Jejak pekerjaan kami di seluruh Indonesia
ProjectsDokumentasi Instalasi Weather Station AWLR Taharica di Blok I22, PT Agro Bukit, SampitBlok I22 · PT Agro Bukit, Sampit Instalasi Weather Station & AWLR di Blok I22 Dari…Sep 2026
ProjectsDokumentasi Instalasi Weather Station AWLR Taharica di Blok M16, PT Nabire Baru, Papua TengahBlok M16 · PT Nabire Baru, Papua Tengah Instalasi Weather Station & AWLR di Blok M16…Sep 2026
ProjectsDokumentasi Instalasi Weather Station AWLR Taharica di Blok C15, PT Rim Capital, SampitBlok C15 · PT Rim Capital, Sampit Instalasi Weather Station & AWLR di Blok C15 Dari…Sep 2026
ProjectsDokumentasi Instalasi Weather Station Taharica di Blok F13 PT Agro BukitBlok F13 · PT Agro Bukit Instalasi Weather Station di Blok F13 Dari lapangan tanpa data…Sep 2026
ProjectsTraining Dan Edukasi Product Fakoop 3D Arborsonic – BRINCibinong, 10 Desember 2025 – Sebagai bentuk komitmen dalam mendukung kemajuan teknologi penelitian di Indonesia, Taharica…Feb 2026Gak ada proyek yang cocok sama pencarian lu.